Magnetics Inc
-
0078083A7
01001012Composition 6.5 SiFe alloy Saturation Flux Density 1.6 Tesla Typical Core Loss (50kHz,100mT) 650 mW/cm3 Curie Temperature 700˚C Operating Temperature Range -30˚C to 200˚
$9.71 -
C058380A2
01001013High Saturation (1.5 T) Lower core loss than Iron Powder or Laminated Silicon Lower cost than MPP material Best DC Bias Very high Curie temperature Stable performance
$8.49